THB spare parts
Here you will find reference materials and sensors for your THB.
Suitable to adjust the contact pressure manually, which improves the contact to the sensor
Suitable for THB/QSS sensors (THB Advance & Ultimate)
Thermal conductivity 1.12 W/mK
Temperature range: -150°C up to 200°C**
Measuring range: 0.01 - 30 W/mK
Suitable for: Solids, Powder, Liquids, Gases
Compatible with: THB Advance, THB Ultimate
* The exact min. sample size depends on the material properties.
** All maximum temperature refer to operation under air. If Kapton Sensors are used in inert atmosphere the maximum temperature range can be extended from 200°C to 300°C.
Measuring range: 0.01 - 5 W/mK
Suitable for: Solids, Powder, Liquids, GasesCompatible with: THB Advance, THB Ultimate
The high temperature (HT) version is based on a ceramic substrate, which slightly reduces the accuracy.
* The exact min. sample size depends on the material properties.
** All maximum temperature refer to operation under air. If Kapton Sensors are used in inert atmosphere the maximum temperature range can be extended from 200°C to 300°C.
Suitable for all THB sensors
Thermal conductivity 0.194 W/mK
Temperature range: RT up to 700°C**
Measuring range: 0.2 - 100 W/mK
Suitable for: Solids, Powder, Liquids
Compatible with: THB Advance, THB Ultimate
The high temperature (HT) version is based on a ceramic substrate, which slightly reduces the accuracy.
* The exact min. sample size depends on the material properties.
** All maximum temperature refer to operation under air. If Kapton Sensors are used in inert atmosphere the maximum temperature range can be extended from 200°C to 300°C.
Temperature range: -150°C up to 200°C**
Measuring range: 0.005 - 1800 W/mK
Suitable for: Solids, Powder
Compatible with: THB Advance, THB Ultimate
* The exact min. sample size depends on the material properties.
** All maximum temperature refer to operation under air. If Kapton Sensors are used in inert atmosphere the maximum temperature range can be extended from 200°C to 300°C.
Compatible with: metal frames
Temperature range: -150°C up to 300°C**
Measuring range: 0.01 - 5 W/mK
Suitable for: Solids
Compatible with: THB Basic, THB Advance, THB Ultimate
* The exact min. sample size depends on the material properties.
** All maximum temperature refer to operation under air. If Kapton Sensors are used in inert atmosphere the maximum temperature range can be extended from 200°C to 300°C.
Temperature range: -150°C up to 300°C**
Measuring range: 0.01 - 5 W/mK
Suitable for: Solids, Powder, Liquids
Compatible with: THB Basic, THB Advance, THB Ultimate
* The exact min. sample size depends on the material properties.
** All maximum temperature refer to operation under air. If Kapton Sensors are used in inert atmosphere the maximum temperature range can be extended from 200°C to 300°C.
Temperature range: -150°C up to 300°C**
Measuring range: 0.01 - 2 W/mK
Suitable for: Solids
Compatible with: THB Basic, THB Advance, THB Ultimate
* The exact min. sample size depends on the material properties.
** All maximum temperature refer to operation under air. If Kapton Sensors are used in inert atmosphere the maximum temperature range can be extended from 200°C to 300°C.
Temperature range: -150°C up to 300°C**
Measuring range: 0.01 - 2 W/mK
Suitable for: Solids, Powder, Liquids
Compatible with: THB Basic, THB Advance, THB Ultimate
* The ecaxt min. sample size depends on the material properties.** All maximum temperature refer to operation under air. If Kapton Sensors are used in inert atmosphere the maximum temperature range can be extended from 200°C to 300°C.
Temperature range: RT up to 700°C**
Measuring range: 0.01 - 1 W/mK
Suitable for: Solids
Compatible with: THB Basic, THB Advance, THB Ultimate
The high temperature (HT) version is based on a ceramic substrate, which slightly reduces the accuracy.
* The exact min. sample size depends on the material properties.
** All maximum temperature refer to operation under air. If Kapton Sensors are used in inert atmosphere the maximum temperature range can be extended from 200°C to 300°C.
Suitable for THB/QSS sensors (THB Advance & Ultimate)
Thermal conductivity 67 W/mK
Suitable for THB/QSS sensors (THB Advance & Ultimate)
Thermal conductivity 22 W/mK
Suitable for THB/QSS sensors (THB Advance & Ultimate)
Thermal conductivity 110 W/mK