For highest accurate measurements up to 1600°CSample diameter max. 12 mm / sample length max. 50 mmIncluded: tube, piston, gas capillare, clips
For highest accurate measurements up to 1600°CSample diameter max. 20 mm / sample length max. 50 mmIncluded: tube, piston, gas capillare, clips
For highest accurate measurements up to 1600°CSample diameter max. 7 mm / sample length max. 50 mmIncluded: tube, piston, gas capillare, clips
For highest accurate measurements up to 1000°CSample diameter max. 12 mm / sample length max. 50 mmIncluded: tube, piston, gas capillare, clips
For highest accurate measurements up to 1000°Csample diameter max. 20 mm / sample length max. 50 mmIncluded: tube, piston, gas capillare, clips
For highest accurate measurements up to 1000°CSample diameter max. 7 mm / sample length max. 50 mmIncluded: tube, piston, gas capillare, clips
Replacement thermocouple type k for sample measurementsFor measurements from -180°C to 700°C
Replacement thermocouple type S for sample measurementsFor measurements from RT to 1600°C
Purity declaration possible on request
Thickness: 2 mmDiameter: 6 mmFor measurements up to 1600°C99,7% purity