Calibration material Tin

Product information

  • Melting temperature: 231.928°C
Skip product gallery

Other calibration materials

Calibration material Zinc
Calibration material Zinc

Melting temperature: 419.527°C

Product number: 02-05-005-305
Calibration material Aluminium
Calibration material Aluminium

Melting temperature: 660.325°C

Product number: 06-400-100-001
Calibration material Palladium
Calibration material Palladium

Melting temperature: 1554°C

Product number: 06-400-100-003
Calibration material Indium
Calibration material Indium

Melting temperature: 156.5985°C

Product number: 02-05-005-302
Calibration material Lead
Calibration material Lead

Melting temperature: 329.462°C

Product number: 02-05-005-304
Calibration material Gold
Calibration material Gold

Melting temperature: 1064.18°C

Product number: 06-400-100-002